Danyang Kaixin Alloy Material Co., Ltd.

Danyang Kaixin Alloy Material Co., Ltd.

Manufacturer from China
Verified Supplier
3 Years
Home / Products / Expansion Alloy /

4J40 Corrosion Resistant Alloy Rod Iron Nickel Cobalt Alloy

Contact Now
Danyang Kaixin Alloy Material Co., Ltd.
Visit Website
Province/State:jiangsu
Country/Region:china
Contact Person:MrsAnnaPei
Contact Now

4J40 Corrosion Resistant Alloy Rod Iron Nickel Cobalt Alloy

Ask Latest Price
Video Channel
Brand Name :KAIXIN
Model Number :KX-Alloy40
Certification :ISO9001:2015
Place of Origin :China
MOQ :200KG
Price :To negotiate
Payment Terms :T/T, L/C
Supply Ability :50~80TONS per MONTH
Delivery Time :45~60days
Packaging Details :Wooden Box, size as per guests's request
Shape :Wire,Strip,Rod,Tube,Plate
Alloy Type :Iron Nickel Cobalt Alloy
Raw Materials :NI32.4-33.4%,CO7-8%,Fe Rem
Executive standard :YB/T 5241
Delivery State :Soft State
Application :To produce a variety of klystron, microwave tube cavity in the electric vacuum industry
Features :Low linear expansion coefficient in the range of 20-100°C and easy to cut machining.
Size :Negotiable
more
Contact Now

Add to Cart

Find Similar Videos
View Product Description

KX 4J40 Corrosion Resistant Alloy Light Rod On Expansion Alloy

Product Description and Application

4J40 is also known as Alloy 40

4J40 is Fe-Ni-Co ternary alloy and its curie point is above 300℃. The alloy has a low expansion coefficient in the temperature range of -20 ~ 300℃, and the transformation from austenite (γ) to martensite (M) does not occur until -60℃. The alloy is mainly used in the manufacture of highly precise instrument parts and electronic devices requiring sizes in the temperature range of -50 to 300℃

Process Performance and Requirements

  • Product Fusion Process

Vacuum Induction Furnace(VIM) and Electroslag Remelting Furnace(ESR)

  • Product Chemical Composition

Alloy Grade Chemical Composition (mass fraction)(%)
C Si P S Mn Cu Ni Co Fe
4J40 0.05 0.15 0.02 0.02 0.25 --- 32.4~33.4 7.0~8.0 Rem

  • Product Linear Expansion Coefficient

Alloy Grade Sample Heat Treatment Institution Average coefficient of linear expansionα(10-6/ K)
20~100℃ 20~300°C
4J40 The semi-finished sample was heated to 840±10°C, hold for 1 hour, water quenched, and then the sample was processed into finished sample. Heat preservation 1 hour at 315±l0℃ with furnace cooling or air cooling ≤2.0

  • Product Typical Average Linear Expansion Coefficient

Alloy Grade

Average Coefficient of Linear Expansion

α(10-6/ K)

20~50℃ 20~100℃ 20~200℃ 20~300℃ 20~400℃ 20~500℃
4J40 1.4 1.3 1.2 1.7 4.5

  • Productive Process

4J40 Corrosion Resistant Alloy Rod Iron Nickel Cobalt Alloy

  • Professional Customization

Cold-drawn Wire ¢0.3~¢18mm(Delivery in rolls or trays)
Hot-Rolling Wire ¢5.5~¢20mm(Delivery in rolls)
Strip thickness 0.1~4.5*width 6~350mm(Supply in rolls or straight strips)
Smooth Forged Rod on a Lathe

¢60~350mm,L800-2500mm

Hot-rolled Burnishing ¢20~80mm,L1000-5000mm
Cold Drawn and Burnishing ¢2.5~18mm,L1000-8000mm
Seamless Tube ¢1~275mm,wall thickness 0.2~30,L1000-8000mm

4J40 Corrosion Resistant Alloy Rod Iron Nickel Cobalt Alloy

4J40 Corrosion Resistant Alloy Rod Iron Nickel Cobalt Alloy4J40 Corrosion Resistant Alloy Rod Iron Nickel Cobalt Alloy4J40 Corrosion Resistant Alloy Rod Iron Nickel Cobalt Alloy4J40 Corrosion Resistant Alloy Rod Iron Nickel Cobalt Alloy

Inquiry Cart 0